General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.4 % Show Supplier Material materials with Absorción de agua of 1.4 % | Sim. to ISO 62 | |
Bio-based content | 44 % Show Supplier Material materials with Bio-based content of 44 % | ||
48 % Show Supplier Material materials with Bio-based content of 48 % | |||
Densidad | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 39 [-] Show Supplier Material materials with Dureza Shore D of 39 [-] | dry | ISO 7619-1 | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. |
Módulo elástico | 0.075 GPa Show Supplier Material materials with Módulo elástico of 0.075 GPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | No Break at 23 and -30°C | cond., dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 148 °C Show Supplier Material materials with Temperatura de fusión of 148 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 121 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 121 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Eyewear Frames,Footwear - Outsoles | |
Processing methods | Injection Molding: Extrusion: |