General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.5 % Show Supplier Material materials with Absorción de agua of 1.5 % | Sim. to ISO 62 | |
Bio-based content | 62 % Show Supplier Material materials with Bio-based content of 62 % | ||
68 % Show Supplier Material materials with Bio-based content of 68 % | |||
Densidad | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 51 [-] Show Supplier Material materials with Dureza Shore D of 51 [-] | dry | ISO 7619-1 | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. |
Límite elástico | 19 MPa Show Supplier Material materials with Límite elástico of 19 MPa | cond. | ISO 527-1/-2 | |
Módulo elástico | 0.16 GPa Show Supplier Material materials with Módulo elástico of 0.16 GPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | No Break at 23 and -30°C | cond., dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 167 °C Show Supplier Material materials with Temperatura de fusión of 167 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 156 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 156 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Tubing and Hoses,Eyewear Frames,Footwear - Outsoles,Ski Boots | |
Processing methods | Injection Molding: Extrusion: |