General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | dry | ISO 1183 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 115 °C Show Supplier Material materials with Temperatura de fusión of 115 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior,Hot Melt Adhesives - Sports Apparel and Underwear,Textile - Others |