Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Platamid® H 2513 Powder
Copolyamide Hot Melt Adhesive / Textile Applications
Platamid® H 2513 Powder is a medium melt viscosity copolyamide adhesive powder for the production of fusible interlinings.
Platamid® H 2513 Powder offers an excellent laundry resistance up to 60°C and an excellent resistance to all kind of steam treatment.
This product is available in different grain sizes:
PACKAGING
Platamid® H 2513 PTA 170 is delivered in 20 kg sealed bags and 500 kg sealed big bags (GRVS). Platamid® H 2513 PA 80 and Platamid ® H 2513 PTA 170/20 are delivered in 20 kg sealed bags.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.
All categories
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 128 °C Show Supplier Material materials with Temperatura de fusión of 128 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 30 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 30 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property |
---|
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.