General
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 110 °C Show Supplier Material materials with Temperatura de fusión of 110 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 6 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 6 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Decorative Films,Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior,Hot Melt Hot Melt Adhesives Flooring - Flooring,Hot Melt Hot Melt Adhesives Interlining / Garments - Interlining / Garments,Circuit Board Adhesives |