Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Platamid® M 1657
Platamid® M 1657
Copolyamide Hot Melt Adhesive / Extrusion Applications
Platamid® M 1657 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This very low melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments.
Platamid® M 1657 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc).
Platamid® M 1657 has a very good dry cleaning resistance and washing resistance up to 40°C.
This product is available:
PACKAGING
Platamid® M 1657 TA is delivered in 25 kg sealed bags. Platamid®M 1657 FA is delivered in 25 kg sealed bags and 500 kg sealed big bags (GRVS). These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.
All categories
General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | dry | ISO 1183 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 107 °C Show Supplier Material materials with Temperatura de fusión of 107 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 200 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 200 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Accessories |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.