Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Platamid® M 1757
Platamid® M 1757 Copolyamide Hot Melt Adhesive / Extrusion Applications
Platamid® M 1757 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This low to medium melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.
Platamid® M 1757 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc).
Platamid® M 1757 has a very good dry cleaning resistance and washing resistance up to 60°C.
This product is available:
PACKAGING
Platamid® M 1757 TA is delivered in 25 kg sealed bags. Platamid®M 1757 FA is delivered in 500 kg sealed big bags (GRVS). These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.
All categories
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 106 °C Show Supplier Material materials with Temperatura de fusión of 106 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 27 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 27 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior,Hot Melt Hot Melt Adhesives Interlining / Garments - Interlining / Garments,Footwear - Uppers,Accessories |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.