General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 25 % Show Supplier Material materials with Bio-based content of 25 % | ||
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Límite elástico | 38 MPa Show Supplier Material materials with Límite elástico of 38 MPa | cond. | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 102 °C Show Supplier Material materials with Temperatura de fusión of 102 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 26 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior |