General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 64 [-] Show Supplier Material materials with Dureza Shore D of 64 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 22 % Show Supplier Material materials with Elongation at yield of 22 % | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.54 GPa Show Supplier Material materials with Módulo elástico of 0.54 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 176 °C Show Supplier Material materials with Temperatura de fusión of 176 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Brake Tubing,Auto - Water Cooling Circuit,Fuel Management - Fuel Lines,Tubing and Hoses | |
Processing methods | Injection Molding: Extrusion: |