Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 65 [-] Show Supplier Material materials with Dureza Shore D of 65 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 26 % Show Supplier Material materials with Elongation at yield of 26 % | dry | ISO 527-1/-2 | ||
Límite elástico | 28 MPa Show Supplier Material materials with Límite elástico of 28 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.585 GPa Show Supplier Material materials with Módulo elástico of 0.585 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 82 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 82 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 174 °C Show Supplier Material materials with Temperatura de fusión of 174 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 1.2 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 1.2 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines,Tubing and Hoses |