General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.6 % Show Supplier Material materials with Absorción de agua of 1.6 % | Sim. to ISO 62 | |
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | ||
7 % Show Supplier Material materials with Elongation at yield of 7 % | cond. | ISO 527-1/-2 | |||
Límite elástico | 34 MPa Show Supplier Material materials with Límite elástico of 34 MPa | cond. | ISO 527-1/-2 | ||
50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | dry | ISO 527-1/-2 | |||
Módulo elástico | 1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | cond. | ISO 527-1/-2 | ||
1.8 GPa Show Supplier Material materials with Módulo elástico of 1.8 GPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
-30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | ||
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 9e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-05 1/K | dry | ISO 11359-1/-2 | |
Temperatura de fusión | 178 °C Show Supplier Material materials with Temperatura de fusión of 178 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 143 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 143 °C | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 7 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 7 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing and Hoses | |
Processing methods | Injection Molding: |