General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.6 % Show Supplier Material materials with Absorción de agua of 1.6 % | Sim. to ISO 62 | |
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond., dry | ISO 527-1/-2 | ||
Límite elástico | 31 MPa Show Supplier Material materials with Límite elástico of 31 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 1.4 GPa Show Supplier Material materials with Módulo elástico of 1.4 GPa | cond. | ISO 527-1/-2 | ||
1.5 GPa Show Supplier Material materials with Módulo elástico of 1.5 GPa | dry | ISO 527-1/-2 | |||
Puncture energy | -30 °C | 60 J Show Supplier Material materials with Puncture energy of 60 J | cond. | ISO 6603-2 | |
Puncture force | -30 °C | 4800 N Show Supplier Material materials with Puncture force of 4800 N | cond. | ISO 6603-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.0001 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0001 1/K | dry | ISO 11359-1/-2 | ||||
Temperatura de fusión | 180 °C Show Supplier Material materials with Temperatura de fusión of 180 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Temperatura de reblandecimiento Vicat | 142 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 142 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB and yellow card available |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | cond. | IEC 60243-1 |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | cond. | IEC 60093 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 8 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 8 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pneumatic Tubing,Tubing and Hoses,Footwear - Outsoles,Accessories,Antitermite Cables,Wire and Cables | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |