General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 69 [-] Show Supplier Material materials with Dureza Shore D of 69 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 6 % Show Supplier Material materials with Elongation at yield of 6 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 37 MPa Show Supplier Material materials with Límite elástico of 37 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 1.4 GPa Show Supplier Material materials with Módulo elástico of 1.4 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 178 °C Show Supplier Material materials with Temperatura de fusión of 178 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.8 % Show Supplier Material materials with Contracción of 0.8 % | dry | ISO 294-4 | |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | dry | ISO 294-4 | Transverse | |
Velocidad de flujo del volumen derretido | 57 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 57 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts,Accessories |