General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 26 MPa Show Supplier Material materials with Límite elástico of 26 MPa | dry | ISO 527-1/-2 | ||
30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | cond. | ISO 527-1/-2 | |||
Módulo elástico | 1.1 GPa Show Supplier Material materials with Módulo elástico of 1.1 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 180 °C Show Supplier Material materials with Temperatura de fusión of 180 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 57 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 57 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,Medical Catheters | |
Certifications | USP Class VI | |
Processing methods | Injection Molding: |