General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.5 % Show Supplier Material materials with Absorción de agua of 1.5 % | Sim. to ISO 62 | |
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | cond. | ISO 527-1/-2 | |
Límite elástico | 105 MPa Show Supplier Material materials with Límite elástico of 105 MPa | cond. | ISO 527-1/-2 | |
116 MPa Show Supplier Material materials with Límite elástico of 116 MPa | dry | ISO 527-1/-2 | ||
Módulo elástico | 9 GPa Show Supplier Material materials with Módulo elástico of 9 GPa | cond. | ISO 527-1/-2 | |
9.6 GPa Show Supplier Material materials with Módulo elástico of 9.6 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | cond. | ISO 527-1/-2 | |
127 MPa Show Supplier Material materials with Resistencia a la tracción of 127 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA |
-30 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | cond., dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 47 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 47 kJ/m² | dry | ISO 179/1eU |
-30 °C | 48 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 48 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry | ISO 179/1eU | |
23 °C | 46 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 46 kJ/m² | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 178 °C Show Supplier Material materials with Temperatura de fusión of 178 °C | dry | ISO 11357-1/-3 | 10°C/min |
Thermal decomposition in air | 223 °C Show Supplier Material materials with Thermal decomposition in air of 223 °C | TGA | 1% wt. loss | |
Thermal decomposition in nitrogen | 223 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 223 °C | TGA | 1% wt. loss |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 100000 Ω/sq Show Supplier Material materials with Surface resistivity of 100000 Ω/sq | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors | |
Fillers | 15% Carbon Fiber | |
Processing methods | Injection Molding: |