General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.3 % Show Supplier Material materials with Absorción de agua of 1.3 % | Sim. to ISO 62 | |
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 5.2 % Show Supplier Material materials with Elongación of 5.2 % | cond. | ISO 527-1/-2 | nominal | |
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | ||
3.5 % Show Supplier Material materials with Elongation at yield of 3.5 % | cond. | ISO 527-1/-2 | |||
Límite elástico | 105 MPa Show Supplier Material materials with Límite elástico of 105 MPa | cond. | ISO 527-1/-2 | ||
127 MPa Show Supplier Material materials with Límite elástico of 127 MPa | dry | ISO 527-1/-2 | |||
Módulo elástico | 5.1 GPa Show Supplier Material materials with Módulo elástico of 5.1 GPa | cond. | ISO 527-1/-2 | ||
5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | ||
100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | cond. | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | |
-30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | cond. | ISO 179/1eA | ||
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 19 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 19 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 66 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 66 kJ/m² | dry | ISO 179/1eU | |
-30 °C | 83 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 83 kJ/m² | cond. | ISO 179/1eU | ||
23 °C | 66 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 66 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 77 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 77 kJ/m² | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 6e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-05 1/K | dry | ISO 11359-1/-2 | |
Temperatura de fusión | 179 °C Show Supplier Material materials with Temperatura de fusión of 179 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 165 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 165 °C | ISO 306 | 50°C/h 50N | |
Thermal decomposition in air | 222 °C Show Supplier Material materials with Thermal decomposition in air of 222 °C | TGA | 1% wt. loss | |
Thermal decomposition in nitrogen | 223 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 223 °C | TGA | 1% wt. loss |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Constante dieléctrica | 5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | dry | 100Hz | IEC 60250 |
5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | dry | 1MHz | IEC 60250 | |
Factor de disipación | 0.0364 [-] Show Supplier Material materials with Factor de disipación of 0.0364 [-] | dry | 1MHz | IEC 60250 |
0.117 [-] Show Supplier Material materials with Factor de disipación of 0.117 [-] | dry | 100Hz | IEC 60250 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 13 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 13 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors | |
Fillers | 23% Glass Fiber | |
Processing methods | Injection Molding: |