General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.3 % Show Supplier Material materials with Absorción de agua of 1.3 % | Sim. to ISO 62 | |
Densidad | 1.24 g/cm³ Show Supplier Material materials with Densidad of 1.24 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | cond. | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongation at yield of 4 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 115 MPa Show Supplier Material materials with Límite elástico of 115 MPa | cond. | ISO 527-1/-2 | |
Módulo elástico | 6.4 GPa Show Supplier Material materials with Módulo elástico of 6.4 GPa | cond. | ISO 527-1/-2 | |
6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | cond. | ISO 527-1/-2 | |
112 MPa Show Supplier Material materials with Resistencia a la tracción of 112 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | cond., dry | ISO 179/1eA |
23 °C | 19 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 19 kJ/m² | cond., dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 83 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 83 kJ/m² | dry, cond. | ISO 179/1eU |
23 °C | 77 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 77 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 79 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 79 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5e-05 1/K | dry | ISO 11359-1/-2 | ||||
Temperatura de fusión | 183 °C Show Supplier Material materials with Temperatura de fusión of 183 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Temperatura de reblandecimiento Vicat | 165 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 165 °C | ISO 306 | 50°C/h 50N | ||||
Thermal decomposition in air | 227 °C Show Supplier Material materials with Thermal decomposition in air of 227 °C | TGA | 1% wt. loss | ||||
Thermal decomposition in nitrogen | 224 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 224 °C | TGA | 1% wt. loss | ||||
Inflamabilidad | At thickness 3.2 mm IEC 60695-11-10: HB and yellow card available |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Constante dieléctrica | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | dry | 1MHz | IEC 60250 |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | 100Hz | IEC 60250 | |
Factor de disipación | 0.0274 [-] Show Supplier Material materials with Factor de disipación of 0.0274 [-] | dry | 1MHz | IEC 60250 |
0.0664 [-] Show Supplier Material materials with Factor de disipación of 0.0664 [-] | dry | 100Hz | IEC 60250 | |
Rigidez dieléctrica | 35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | cond., dry | IEC 60243-1 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | cond. | IEC 60093 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 7 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 7 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts | |
Certifications | Yellow Card | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |