General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.28 g/cm³ Show Supplier Material materials with Densidad of 1.28 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.8 % Show Supplier Material materials with Moisture absorption of 0.8 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
Límite elástico | 25 MPa Show Supplier Material materials with Límite elástico of 25 MPa | dry | ISO 527-1/-2 | |
Módulo elástico | 7.8 GPa Show Supplier Material materials with Módulo elástico of 7.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 137 MPa Show Supplier Material materials with Resistencia a la tracción of 137 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | dry | ISO 179/1eA |
23 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 210 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 210 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts | |
Fillers | 30% Glass Fiber |