General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 1.12 - 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.12 - 1.18 g/cm³ | ISO 1183 | relative density |
Mecánica
Property | Value | Testing Standard |
---|---|---|
Impact energy, coating | 160 J Show Supplier Material materials with Impact energy, coating of 160 J | ASTM D2794 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard |
---|---|---|---|
Temperatura de fusión | 183 - 193 °C Show Supplier Material materials with Temperatura de fusión of 183 - 193 °C | dry | ISO 1218 |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Rigidez dieléctrica | 300 - 1100 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 300 - 1100 kV/mm | ASTM D149 | thickness = 330mm |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Coatings - General Purpose,Powder Coatings - Healthcare,Powder Coatings - Wire Goods | |
Color | Brown | |
Covering efficiency | 0.35 kg/m² | |
Covering efficiency, thickness | 300 µm |