General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 0.8 % Show Supplier Material materials with Absorción de agua of 0.8 % | Sim. to ISO 62 | |
Densidad | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 21 % Show Supplier Material materials with Elongation at yield of 21 % | cond. | ISO 527-1/-2 | |
Límite elástico | 42 MPa Show Supplier Material materials with Límite elástico of 42 MPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | No Break at 23 and -30°C | cond. | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 172 °C Show Supplier Material materials with Temperatura de fusión of 172 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | Medical | |
Processing methods | Extrusion: |