General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 75 % Show Supplier Material materials with Bio-based content of 75 % | ||
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | dry | ISO 1183 |
Mecánica
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 189 °C Show Supplier Material materials with Temperatura de fusión of 189 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed. Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services. | |
Processing methods | Extrusion: |