General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.8 % Show Supplier Material materials with Absorción de agua of 1.8 % | Sim. to ISO 62 | |
Bio-based content | 92 % Show Supplier Material materials with Bio-based content of 92 % | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 33 % Show Supplier Material materials with Elongation at yield of 33 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 32 MPa Show Supplier Material materials with Límite elástico of 32 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.56 GPa Show Supplier Material materials with Módulo elástico of 0.56 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 70 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 182 °C Show Supplier Material materials with Temperatura de fusión of 182 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Brakebooster Lines,Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Pneumatic Tubing | |
Processing methods | Injection Molding: Extrusion: |