General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.7 % Show Supplier Material materials with Absorción de agua of 1.7 % | Sim. to ISO 62 | |
Bio-based content | 85 % Show Supplier Material materials with Bio-based content of 85 % | ||
Densidad | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 71 [-] Show Supplier Material materials with Dureza Shore D of 71 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 2.1 GPa Show Supplier Material materials with Módulo elástico of 2.1 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 186 °C Show Supplier Material materials with Temperatura de fusión of 186 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 162 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 162 °C | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 55 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 55 kV/mm | cond. | IEC 60243-1 |
Surface resistivity | 6e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 6e+13 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 5e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 5e+11 Ω·cm | cond. | IEC 60093 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 1 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 1 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed. Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services. | |
Fillers | 10% Carbon Black | |
Processing methods | Injection Molding: Extrusion: |