General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1 g/cm³ Show Supplier Material materials with Densidad of 1 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 49 [-] Show Supplier Material materials with Dureza Shore D of 49 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | |
Límite elástico | 40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.19 GPa Show Supplier Material materials with Módulo elástico of 0.19 GPa | cond. | ISO 527-1/-2 | ||
Resistencia a la tracción | 36 MPa Show Supplier Material materials with Resistencia a la tracción of 36 MPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 182 °C Show Supplier Material materials with Temperatura de fusión of 182 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore Flexible Pipes |