General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.8 % Show Supplier Material materials with Absorción de agua of 1.8 % | Sim. to ISO 62 | |
Bio-based content | 93 % Show Supplier Material materials with Bio-based content of 93 % | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 64 [-] Show Supplier Material materials with Dureza Shore D of 64 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 40 % Show Supplier Material materials with Elongation at yield of 40 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 29 MPa Show Supplier Material materials with Límite elástico of 29 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.51 GPa Show Supplier Material materials with Módulo elástico of 0.51 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 0.0001 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0001 1/K | dry | ISO 11359-1/-2 | |
Temperatura de fusión | 182 °C Show Supplier Material materials with Temperatura de fusión of 182 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 146 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 146 °C | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 24 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24 kV/mm | cond. | IEC 60243-1 |
Surface resistivity | 2e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+12 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 2 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Brakebooster Lines,Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Pneumatic Tubing,Offshore Oil Production - Anti Wear Tapes | |
Processing methods | Injection Molding: Extrusion: |