General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.6 % Show Supplier Material materials with Absorción de agua of 1.6 % | Sim. to ISO 62 | |
Bio-based content | 89 % Show Supplier Material materials with Bio-based content of 89 % | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 60 [-] Show Supplier Material materials with Dureza Shore D of 60 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 50 % Show Supplier Material materials with Elongation at yield of 50 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 26 MPa Show Supplier Material materials with Límite elástico of 26 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.345 GPa Show Supplier Material materials with Módulo elástico of 0.345 GPa | cond. | ISO 527-1/-2 | ||
Puncture energy | -30 °C | 70 J Show Supplier Material materials with Puncture energy of 70 J | cond. | ISO 6603-2 | |
Puncture force | -30 °C | 6000 N Show Supplier Material materials with Puncture force of 6000 N | cond. | ISO 6603-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00011 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00011 1/K | dry | ISO 11359-1/-2 | |
Temperatura de fusión | 181 °C Show Supplier Material materials with Temperatura de fusión of 181 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 140 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 140 °C | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | 1MHz | IEC 60250 |
9 [-] Show Supplier Material materials with Constante dieléctrica of 9 [-] | dry | 100Hz | IEC 60250 | |
Factor de disipación | 0.104 [-] Show Supplier Material materials with Factor de disipación of 0.104 [-] | dry | 1MHz | IEC 60250 |
0.244 [-] Show Supplier Material materials with Factor de disipación of 0.244 [-] | dry | 100Hz | IEC 60250 | |
Rigidez dieléctrica | 23 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 23 kV/mm | cond. | IEC 60243-1 | |
Surface resistivity | 5e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5e+11 Ω/sq | cond. | IEC 60093 | |
Volume resistivity | 1e+09 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+09 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 3 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3 cm³/10min | dry | ISO 1133 | 235°C/10kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Brake Tubing,Fluid Management - Brakebooster Lines,Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Monofilaments,Pneumatic Tubing,Tubing and Hoses,Sports Equipment,Performance Wire,Wire and Cables | |
Processing methods | Injection Molding: Extrusion: |