General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 85 % Show Supplier Material materials with Bio-based content of 85 % | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 60 [-] Show Supplier Material materials with Dureza Shore D of 60 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 46 % Show Supplier Material materials with Elongation at yield of 46 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 26 MPa Show Supplier Material materials with Límite elástico of 26 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.31 GPa Show Supplier Material materials with Módulo elástico of 0.31 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 182 °C Show Supplier Material materials with Temperatura de fusión of 182 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered dried in sealed packaging (25 kg bags, 550 kg rigid containers) ready to be processed. Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services. | |
Processing methods | Extrusion: |