General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 79 % Show Supplier Material materials with Bio-based content of 79 % | ||
Densidad | 1.11 g/cm³ Show Supplier Material materials with Densidad of 1.11 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 41 % Show Supplier Material materials with Elongation at yield of 41 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 38 MPa Show Supplier Material materials with Límite elástico of 38 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.54 GPa Show Supplier Material materials with Módulo elástico of 0.54 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Temperatura de fusión | 180 °C Show Supplier Material materials with Temperatura de fusión of 180 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-2 and yellow card available |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing and Hoses | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |