General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 97 % Show Supplier Material materials with Bio-based content of 97 % | ||
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 73 [-] Show Supplier Material materials with Dureza Shore D of 73 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 26 % Show Supplier Material materials with Elongación of 26 % | cond. | ISO 527-1/-2 | ||
Módulo elástico | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | cond. | ISO 527-1/-2 | ||
Resistencia a la tracción | 56 MPa Show Supplier Material materials with Resistencia a la tracción of 56 MPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7.8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.8 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 189 °C Show Supplier Material materials with Temperatura de fusión of 189 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Chemical Process Industry - Injection Molding,Footwear - Outsoles,Sports Equipment | |
Fillers | 8% Glass Fiber | |
Processing methods | Injection Molding: |