General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 4 % Show Supplier Material materials with Absorción de agua of 4 % | Sim. to ISO 62 | |
Bio-based content | 45 % Show Supplier Material materials with Bio-based content of 45 % | ||
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 78 [-] Show Supplier Material materials with Dureza Shore D of 78 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 61 MPa Show Supplier Material materials with Límite elástico of 61 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 1.7 GPa Show Supplier Material materials with Módulo elástico of 1.7 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.5 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Temperatura de transición del vidrio | 150 °C Show Supplier Material materials with Temperatura de transición del vidrio of 150 °C | dry | ISO 11357-1/-2 | 10°C/min | |||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-2 and yellow card available |
Óptico
Property | Value | Testing Standard |
---|---|---|
Transmisión lumínica | 92 [-] Show Supplier Material materials with Transmisión lumínica of 92 [-] | ISO 13468-1/2 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Eyewear Frames | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |