General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Absorción de agua | 1.9 % Show Supplier Material materials with Absorción de agua of 1.9 % | Sim. to ISO 62 | |
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | relative density |
Median particles size | 27 - 31 μm Show Supplier Material materials with Median particles size of 27 - 31 μm | ISO 13320 | |
Non Tap density | 0.37 g/cm³ Show Supplier Material materials with Non Tap density of 0.37 g/cm³ | ISO 1068 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Temperatura de fusión | 185 °C Show Supplier Material materials with Temperatura de fusión of 185 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Temperatura de reblandecimiento Vicat | 160 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 160 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: V-2 |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | dry | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered in 20kg bag. Shelf Life** Five years from the date of delivery. For any use after this limit, please refer to our technical services. |