Property | Value | Testing Standard | Comment |
---|---|---|---|
Absorción de agua | 1 % Show Supplier Material materials with Absorción de agua of 1 % | ISO 62-1 | max. | for 24h |
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | relative density |
Median particles size | 43 - 55 μm Show Supplier Material materials with Median particles size of 43 - 55 μm | ISO 13320 | |
Non Tap density | 0.38 g/cm³ Show Supplier Material materials with Non Tap density of 0.38 g/cm³ | ISO 1068 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard |
---|---|---|---|
Temperatura de fusión | 186 °C Show Supplier Material materials with Temperatura de fusión of 186 °C | dry | ISO 1218 |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered in 20kg bag. Shelf Life** Five years from the date of delivery. For any use after this limit, please refer to our technical services. |