General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.9 % Show Supplier Material materials with Absorción de agua of 1.9 % | Sim. to ISO 62 | |
Densidad | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | ISO 1183 | dry |
Median particles size | 30 μm Show Supplier Material materials with Median particles size of 30 μm | ISO 13320 | |
Non Tap density | 0.43 g/cm³ Show Supplier Material materials with Non Tap density of 0.43 g/cm³ | ISO 1068 | |
Tap density | 0.63 g/cm³ Show Supplier Material materials with Tap density of 0.63 g/cm³ | ISO 1068 |
Mecánica
Property | Value | Testing Standard | |
---|---|---|---|
Hardness, Persoz | 270 [-] Show Supplier Material materials with Hardness, Persoz of 270 [-] | ISO 1522 | |
Hardness, Pencil test | ECCA T4: B |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de reblandecimiento Vicat | 160 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 160 °C | ISO 306 | 50°C/h 50N | ||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: V-2 |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | dry | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Coatings - Automotive & Transportation,Powder Coatings - General Purpose | |
Color | Black | |
Covering efficiency | 0.2 kg/m² | |
Covering efficiency, thickness | 100 µm |