General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 1 % Show Supplier Material materials with Absorción de agua of 1 % | ISO 62-1 | max. | for 24h | |
Bio-based content | 59 % Show Supplier Material materials with Bio-based content of 59 % | |||
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongation at yield | 39 % Show Supplier Material materials with Elongation at yield of 39 % | cond. | ISO 527-1/-2 | |
Límite elástico | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | cond. | ISO 527-1/-2 | |
Módulo elástico | 0.54 GPa Show Supplier Material materials with Módulo elástico of 0.54 GPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | cond. | ISO 179/1eA |
23 °C | 24 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 24 kJ/m² | cond. | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Processing methods | Extrusion: |