General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 53 % Show Supplier Material materials with Bio-based content of 53 % | ||
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | cond. | ISO 527-1/-2 | |
Límite elástico | 37 MPa Show Supplier Material materials with Límite elástico of 37 MPa | dry | ISO 527-1/-2 | |
Módulo elástico | 7.6 GPa Show Supplier Material materials with Módulo elástico of 7.6 GPa | cond. | ISO 527-1/-2 | |
Resistencia a la tracción | 151 MPa Show Supplier Material materials with Resistencia a la tracción of 151 MPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | cond. | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | cond. | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 32 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 32 kJ/m² | cond. | ISO 179/1eU |
23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 255 °C Show Supplier Material materials with Temperatura de fusión of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 12 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 12 cm³/10min | dry | ISO 1133 | 275°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors | |
Fillers | 15% Carbon Fiber | |
Processing methods | Injection Molding: |