General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.13 % Show Supplier Material materials with Absorción de agua of 1.13 % | Sim. to ISO 62 | |
Bio-based content | 67 % Show Supplier Material materials with Bio-based content of 67 % | ||
Densidad | 1.3 g/cm³ Show Supplier Material materials with Densidad of 1.3 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.22 % Show Supplier Material materials with Moisture absorption of 0.22 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 83 [-] Show Supplier Material materials with Dureza Shore D of 83 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | cond. | ISO 527-1/-2 | ||
Límite elástico | 45 MPa Show Supplier Material materials with Límite elástico of 45 MPa | dry | ISO 527-1/-2 | ||
Módulo elástico | 8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | cond. | ISO 527-1/-2 | ||
Resistencia a la tracción | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 46 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 46 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 51 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 51 kJ/m² | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 255 °C Show Supplier Material materials with Temperatura de fusión of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | dry | ISO 1133 | 300°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Auto - Water Cooling Circuit | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |