General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 40 % Show Supplier Material materials with Elongation at yield of 40 % | cond. | ISO 527-1/-2 | |
Límite elástico | 33 MPa Show Supplier Material materials with Límite elástico of 33 MPa | cond. | ISO 527-1/-2 | |
Módulo elástico | 0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | cond. | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 4.6 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 4.6 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines | |
Processing methods | Extrusion: |