General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 2.9 % Show Supplier Material materials with Absorción de agua of 2.9 % | Sim. to ISO 62 | |
Densidad | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 31 % Show Supplier Material materials with Elongation at yield of 31 % | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.515 GPa Show Supplier Material materials with Módulo elástico of 0.515 GPa | cond. | ISO 527-1/-2 | ||
0.685 GPa Show Supplier Material materials with Módulo elástico of 0.685 GPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.5 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 95 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 95 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 3.7 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3.7 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - In-Tank and Fuel Venting Lines | |
Processing methods | Extrusion: |