General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 3.92 g/cm³ Show Supplier Material materials with Densidad of 3.92 g/cm³ | |
Rugosidad superficial | 3.6 μm Show Supplier Material materials with Rugosidad superficial of 3.6 μm | Rz* |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 1733 [-] Show Supplier Material materials with Dureza Vickers of 1733 [-] | converted from GPa |
Módulo elástico | 23.0 °C | 380 GPa Show Supplier Material materials with Módulo elástico of 380 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 4.3 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4.3 MPa·√m | |
Resistencia a la compresión | 23.0 °C | 2800 MPa Show Supplier Material materials with Resistencia a la compresión of 2800 MPa | |
Resistencia a la flexión | 23.0 °C | 440 MPa Show Supplier Material materials with Resistencia a la flexión of 440 MPa | 4-point bending flexural test |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8E-6 1/K |
Conductividad térmica | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.00E+14 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+14 Ω·m |
600.0 °C | 1000000 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1000000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Wear parts for the textile and the machine engineering industry Suitable for high temperatures and corrosive environments, e.g. in laboratories Insulating parts for electronics and electrical engineering | |
Other | *depending on the processing status of the injection molding or pressing tool | |
Processing history | Ceramic Injection Molding (CIM) |