Medidas
Property | Value |
---|---|
Espesor | 5 - 15 mm Show Supplier Material materials with Espesor of 5 - 15 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Brinell of 95 [-] |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Elongación A50 | 23.0 °C | 8 % Show Supplier Material materials with Elongación A50 of 8 % |
Límite elástico Rp 0,2 | 23.0 °C | 260 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 260 MPa |
Resistencia a la tracción | 23.0 °C | 310 MPa Show Supplier Material materials with Resistencia a la tracción of 310 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | balance |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Cromo | 0.25 % Show Supplier Material materials with Cromo of 0.25 % |
Hierro | 0.5 % Show Supplier Material materials with Hierro of 0.5 % |
Magnesio | 0.6 - 1.2 % Show Supplier Material materials with Magnesio of 0.6 - 1.2 % |
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % |
Silicona | 0.7 - 1.3 % Show Supplier Material materials with Silicona of 0.7 - 1.3 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Zinc | 0.2 % Show Supplier Material materials with Zinc of 0.2 % |