Medidas
Property | Value |
---|---|
Espesor | 10 mm Show Supplier Material materials with Espesor of 10 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 75 [-] Show Supplier Material materials with Dureza Brinell of 75 [-] |
Elongación | 23.0 °C | 8 % Show Supplier Material materials with Elongación of 8 % |
Elongación A50 | 23.0 °C | 6 % Show Supplier Material materials with Elongación A50 of 6 % |
Límite elástico Rp 0,2 | 23.0 °C | 170 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 170 MPa |
Resistencia a la tracción | 23.0 °C | 215 MPa Show Supplier Material materials with Resistencia a la tracción of 215 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | balance |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.35 % Show Supplier Material materials with Hierro of 0.35 % |
Magnesio | 0.45 - 0.9 % Show Supplier Material materials with Magnesio of 0.45 - 0.9 % |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % |
Silicona | 0.2 - 0.6 % Show Supplier Material materials with Silicona of 0.2 - 0.6 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |