Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 20 [-] Show Supplier Material materials with Dureza Brinell of 20 [-] |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % |
Elongación A50 | 23.0 °C | 23 % Show Supplier Material materials with Elongación A50 of 23 % |
Límite elástico Rp 0,2 | 23.0 °C | 20 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 20 MPa |
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 99.5 % Show Supplier Material materials with Aluminio of 99.5 % |
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % |
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % |
Magnesio | 0.05 % Show Supplier Material materials with Magnesio of 0.05 % |
Manganeso | 0.05 % Show Supplier Material materials with Manganeso of 0.05 % |
Otro | 0.03 % Show Supplier Material materials with Otro of 0.03 % |
Silicona | 0.25 % Show Supplier Material materials with Silicona of 0.25 % |
Titanio | 0.05 % Show Supplier Material materials with Titanio of 0.05 % |
Zinc | 0.07 % Show Supplier Material materials with Zinc of 0.07 % |
Technological properties
Property | ||
---|---|---|
Coating | suitable for electro-chemical brightening and anodizing | |
Corrosion properties | corrosion resistant | |
Processing methods | Excellent forming properties | |
Welding | weldable |