General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.9042 g/cm³ Show Supplier Material materials with Densidad of 0.9042 g/cm³ | Exact value: 0.90424 |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 3.3E-3 GPa Show Supplier Material materials with Módulo elástico of 3.3E-3 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.9E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.9E-4 1/K | |
Temperatura de transición del vidrio | -50 °C Show Supplier Material materials with Temperatura de transición del vidrio of -50 °C | max. | |
Temperatura máx. de funcionamiento | 350 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 350 °C | decomposition temperature |
Technological properties
Property | ||
---|---|---|
Application areas | High temperature adhesives and bonding |