Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
BrewerBOND® 701
High temperature stable laser debond material. Polar solvent system with low stress (zero force) debonding for high temperature process and ultrathin samples
Los datos sobre este material han sido proporcionados por Brewer Science.
All categories
Medidas
Property | Value | Comment |
---|---|---|
Espesor | 1.5E-4 mm Show Supplier Material materials with Espesor of 1.5E-4 mm | Nominal coat thickness |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura máx. de funcionamiento | 400 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 400 °C |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Viscosidad | 23.0 °C | 7 Pa·s Show Supplier Material materials with Viscosidad of 7 Pa·s |
Technological properties
Property | ||
---|---|---|
Application areas | High temperature temporary adhesives and bonding |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.