Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de transición del vidrio | 42 - 158 °C Show Supplier Material materials with Temperatura de transición del vidrio of 42 - 158 °C | respectively for before and after cross linking (205°C/60s bake) |
Temperatura máx. de funcionamiento | 290 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 290 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Surface Planarization, High Temperature Gap fill, Spin-on Carbon, High temperature thermoset, Semiconductor Industry, Aerospace, Automotive, Packaging, Electronic Packaging |