Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.45E-4 - 2.35E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.45E-4 - 2.35E-4 1/K | respectively for below and above Tg |
Temperatura de transición del vidrio | 178 °C Show Supplier Material materials with Temperatura de transición del vidrio of 178 °C | ||
Temperatura máx. de funcionamiento | 300 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 300 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Surface Planarization, High Temperature Gap fill, Spin-on Carbon, High temperature thermoset, Semiconductor Industry, Aerospace, Automotive, Packaging, Electronic Packaging |