General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 - 0.94 g/cm³ Show Supplier Material materials with Densidad of 0.92 - 0.94 g/cm³ | ISO 1183/ISO 1872-2B |
Mecánica
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Brittleness temperature | -70 °C Show Supplier Material materials with Brittleness temperature of -70 °C | Max., ASTM D746 |
Temperatura de fusión | 125 °C Show Supplier Material materials with Temperatura de fusión of 125 °C | Min., ISO 3146 |
Temperatura de reblandecimiento Vicat | 90 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 90 °C | Min., ISO 306 A-50, ASTM D 746 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 1.4 - 2.2 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 1.4 - 2.2 g/10min | ISO 1133, 190°С/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | METALEN APE-1 is recommended for the top coat of pipe insulation by side or circular (longitudinal) extrusion. | |
Processing methods | METALEN APE-1 is recommended to be processes on extruders with a flat or circular die. METALEN APE 1 ensures good processability in wide temperature range. The below conditions may be used when starting the extruder: Barrel: 190–230°C, Head: 190–230°C, Die: 220–225°C, Melt temperature: 220–225°C. Definitive processing recommendations may only be given when the specific material application and the equipment type used are known. |