Material: el 'Grade 310 Stainless Steel' que buscabas ha sido remplazado por el material siguiente.

Grade 310 Stainless Steel

View suppliers (24)
Want to keep this datasheet? Save it now in your required format

Description

1.4841 (X15CrNiSi25-21) is an austenitic heat-resisting stainless steel. It is noted for excellent resistance to scaling in continuous service up to 1150°C, and in intermittent heating/cooling conditions up to 1095°C. This grade is highly resistant to oxidising acids and most common corrosive agents, and in marine conditions it shows little evidence of chloride stress corrosion cracking, outperforming lower alloy grades such as 304 and 316. In particular it has good resistance to hot corrosion in many environments including molten salts. It shows the following features and properties:


  • Oxidation resistance to 1150°C
  • Excellent corrosion resistance
  • High strength
  • Strength and toughness at sub-zero temperatures
  • Related Standards

    Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    Propiedades

    Mecánica

    PropertyTemperatureValue

    Elongación

    23.0 °C

    40 %

    Show Material materials with Elongación of 40 %

    Límite elástico

    23.0 °C

    205 MPa

    Show Material materials with Límite elástico of 205 MPa

    Resistencia a la tracción

    23.0 °C

    510 MPa

    Show Material materials with Resistencia a la tracción of 510 MPa

    Chemical properties

    PropertyValue

    Cromo

    25 %

    Show Material materials with Cromo of 25 %

    Hierro

    Balance

    Níquel

    20 %

    Show Material materials with Níquel of 20 %

    Technological properties

    Property
    Application areas

    Aerospace: Aircraft and jet engine components;Chemical processing: Chemical plant and equipment, fasteners for elevated temperature work, mufflers, heat exchangers and components for high temperature sulphur-bearing environments;Other: Oven linings, boiler baffles, kilns, lead pots, radiant tubes, annealing covers, burners, combustion tubes, refractory anchor bolts, fire box sheets, furnace components and other high temperature containers

    Corrosion properties

    Excellent corrosion resistance