1.4542 (X5CrNiCuNb16-4) is a well-established precipitation hardening martensitic stainless steel capable of achieving very high strength and hardness after a relatively simple heat treatment. It offers excellent corrosion resistance combined with a structured range of mechanical property levels depending on the precise heat treatment applied. It is readily machined and fabricated in the softer tempers and can then be heat-treated to exceptional strength and dimensional stability. It shows the following features and properties:


  • Very high strength
  • Very good resistance to pitting and crevice corrosion
  • Excellent resistance to chloride stress corrosion cracking
  • Good workability and weldability
  • Related Standards

    Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    Propiedades

    Chemical properties

    PropertyValueComment

    Cobre

    4 %

    Show Material materials with Cobre of 4 %

    Cromo

    17 %

    Show Material materials with Cromo of 17 %

    Hierro

    Balance

    Niobio

    0.3 %

    Show Material materials with Niobio of 0.3 %

    Nb+Ta

    Níquel

    4 %

    Show Material materials with Níquel of 4 %

    Tántalo

    0.3 %

    Show Material materials with Tántalo of 0.3 %

    Nb+Ta

    Technological properties

    Property
    Application areas

    Offshore & marine: Offshore foils, helicopter deck platforms, pump shafts, couplings, fasteners, valve parts and spindles;Aerospace: Turbine blades, missile and rocket fittings, undercarriage components and fasteners;Other: Nuclear waste casks, medical instruments, paper mill equipment and chemical process plant, springs, screws, bolts, gears, bushes and wear rings

    Corrosion properties

    Very high corrosion resistance

    General machinability

    It is readily machinable