Medidas
Property | Value |
---|---|
Diámetro | 5 - 40 mm Show Supplier Material materials with Diámetro of 5 - 40 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 220 [-] Show Supplier Material materials with Dureza Brinell of 220 [-] | soft annealed |
Dureza Rockwell C | 58 - 62 [-] Show Supplier Material materials with Dureza Rockwell C of 58 - 62 [-] |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.27e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.27e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.37e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.37e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.42e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.42e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.49e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.49e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.58e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.58e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.68e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.68e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 34.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 34.2 W/(m·K) | |
350 °C | 32.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 32.6 W/(m·K) | ||
700 °C | 31 W/(m·K) Show Supplier Material materials with Conductividad térmica of 31 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 1.2 % Show Supplier Material materials with Carbono of 1.2 % |
Cromo | 0.7 % Show Supplier Material materials with Cromo of 0.7 % |
Hierro | Balance |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Piercing dies, guide rods, twist drills, ejector pins and wood chisels | |
Heat Treatment | Soft annealing: 710-750°C (Cooling in furnace) - Stress-relief-annealing: 650-680°C, Hardening: 810-840°C (in oil) 780-810°C (in water) |